Co-Cr disc for milling ceramic-veneered crowns and bridges.

 

Advantages:

  • lower hardness 255 HV10 which facilitates milling and reduces wear of cutters;
  • pure oxidation;
  • coefficient of thermal expansion appropriate for most ceramic materials.

 

Mesa Magnum Solare Co-Cr disc

₪750.00Price
Quantity
  • Composition in %:

    • What 66;
    • Cr 27;
    • Mo 6;
    • Si,Mn 1.

     

    Technical Data:

    • melting point 1307°C - 1417 °C;
    • thermal expansion coefficient - (25- 500 °C) 14.3 x10- 6K- 1 - (25- 600°C) 14.5x10- 6K- 1;
    • density - 8.4g/cm3;
    • Vickers hardness 255 HV10;
    • percentage elongation at break 11%;
    • unit yield strength - 395 Mpa;
    • modulus of elasticity 233 GPa.

     